It is applied for production operations of metal processing by chip removal, which is used for the machining of steel and gray iron. It is especially suitable for individual systems exposed to frequent pollution.
Mineral oil content (%) | 12 |
Density at 20 ºC (g/mL) | 1,030 |
pH-value (3.5% in water) | 9,3 |
Chip/filter paper corrosion test (3.5% in 20°dH water) | 0/0 |
Package | 20L 180 kg |
Choose a product